Method for preparing methyl alcohol, formaldehyde and CO used for methane direct selective oxidation
The invention discloses a method for preparing methyl alcohol, formaldehyde and CO used for methane direct selective oxidation. The method comprises the following steps: preparing a BN powder materialcatalyst, after mixing boric acid with urea, dissolving and stirring with a water and methyl alcohol...
Saved in:
| Main Authors | , , , , , |
|---|---|
| Format | Patent |
| Language | Chinese English |
| Published |
27.02.2018
|
| Subjects | |
| Online Access | Get full text |
Cover
| Summary: | The invention discloses a method for preparing methyl alcohol, formaldehyde and CO used for methane direct selective oxidation. The method comprises the following steps: preparing a BN powder materialcatalyst, after mixing boric acid with urea, dissolving and stirring with a water and methyl alcohol mixed solvent, carrying out thermostatic waterbath standing for crystallization, and roasting under an inert atmosphere to obtain a BN powder material; tabletting and forming a roasted sample, smashing and sieving to obtain a BN powder material catalyst; catalyst activation: introducing oxygen-containing gas into a continuous flow reactor filled with the BN powder material catalyst for heating, activating, introducing inert gas, adjusting to a reaction temperature, and switching into a reaction gas; and preparing methyl alcohol, formaldehyde and CO.
种用于甲烷直接选择氧化制备甲醇、甲醛、CO的方法,涉及甲烷。制备BN粉末材料催化剂,将硼酸和尿素混合后,用水和甲醇混合溶剂溶解、搅拌后,恒温水浴静置进行晶化,在惰性气氛下焙烧,得BN粉末材料;将焙烧样品压片成型,粉碎,过筛,得BN粉末材料催化剂;催化剂活化:将含氧气体通入装有BN粉末材料催化剂的连续流动反应器中加热,活化,通入惰性气 |
|---|---|