EVALUATION OF DUCTILE FRACTURE CRITERIA IN A GENERAL THREE-DIMENSIONAL STRESS STATE CONSIDERING THE STRESS TRIAXIALITY AND THE LODE PARAMETER
This paper is concerned with evaluation of various ductile fracture criteria in a general three-dimensional stress state of stress triaxiality, the Lode parameter and the equivalent plastic strain to fracture. Evaluation is carried out by comparing fracture loci constructed by fracture criteria to e...
Saved in:
| Published in | Acta mechanica solida Sinica Vol. 26; no. 6; pp. 642 - 658 |
|---|---|
| Main Authors | , |
| Format | Journal Article |
| Language | English |
| Published |
Singapore
Elsevier Ltd
01.12.2013
Springer Singapore School of Mechanical, Aerospace and Systems Engineering, KAIST, 335, Gwahangno, Daeduk Science Town,Daejeon, 305-701, South Korea |
| Subjects | |
| Online Access | Get full text |
| ISSN | 0894-9166 1860-2134 |
| DOI | 10.1016/S0894-9166(14)60008-2 |
Cover
| Summary: | This paper is concerned with evaluation of various ductile fracture criteria in a general three-dimensional stress state of stress triaxiality, the Lode parameter and the equivalent plastic strain to fracture. Evaluation is carried out by comparing fracture loci constructed by fracture criteria to experimental results of Al2024-T351. Comparison demonstrates that the Modified Mohr-Coulomb criterion and a newly proposed criterion provide sufficient predictability of fracture strain. Moreover, evaluation is emphasized on the predicted cut-off value for stress triaxiality. The evaluation demonstrates that the Cockcroft-Latham, Brozzo, Oh, Ko-Huh and the new criteria coupled a reasonable cut-off value for ductile materials. |
|---|---|
| Bibliography: | Yanshan Lou,Hoon Huh (School of Mechanical, Aerospace and Systems Engineering, KAIST, 335, Gwahangno, Daeduk Science Town, Daejeon, 305-701, South Korea) 42-1121/O3 This paper is concerned with evaluation of various ductile fracture criteria in a general three-dimensional stress state of stress triaxiality, the Lode parameter and the equiva- lent plastic strain to fracture. Evaluation is carried out by comparing fracture loci constructed by fracture criteria to experimental results of A12024-T351. Comparison demonstrates that the Modified Mohr-Coulomb criterion and a newly proposed criterion provide sufficient predictabil- ity of fracture strain. Moreover, evaluation is emphasized on the predicted cut-off value for stress triaxiality. The evaluation demonstrates that the Cockcroft-Latham, Brozzo, Oh, Ko-Huh and the new criteria coupled a reasonable cut-off value for ductile materials. fracture, alloys, ductile material, fracture locus, metal forming ObjectType-Article-2 SourceType-Scholarly Journals-1 ObjectType-Feature-1 content type line 23 |
| ISSN: | 0894-9166 1860-2134 |
| DOI: | 10.1016/S0894-9166(14)60008-2 |