Formation of Ferrogabbro Through Fe-Ti Oxide Accumulation Under Moderate Oxidation Conditions: Insights from the Dashanshu Intrusion in the Emeishan Large Igneous Province, SW China
The mechanism of iron enrichment in ferrogabbro remains a controversial subject. This study provides valuable insights derived from the Dashanshu intrusion, located in the Emeishan Large Igneous Province in southwestern China, which features ferrogabbro with a notably high iron content (total Fe2O3...
        Saved in:
      
    
          | Published in | Minerals (Basel) Vol. 14; no. 11; p. 1156 | 
|---|---|
| Main Authors | , , , | 
| Format | Journal Article | 
| Language | English | 
| Published | 
        Basel
          MDPI AG
    
        01.11.2024
     | 
| Subjects | |
| Online Access | Get full text | 
| ISSN | 2075-163X 2075-163X  | 
| DOI | 10.3390/min14111156 | 
Cover
| Summary: | The mechanism of iron enrichment in ferrogabbro remains a controversial subject. This study provides valuable insights derived from the Dashanshu intrusion, located in the Emeishan Large Igneous Province in southwestern China, which features ferrogabbro with a notably high iron content (total Fe2O3 reaching up to 21.6 wt.%). The ferrogabbro samples exhibit distinctive petrographic features, including the early crystallization of plagioclase prior to pyroxenes, amphibole replacing pyroxenes, and magnetite–ilmenite intergrowth filling the interstices between plagioclase and pyroxenes. A quantitative mineral analysis based on micro-X-ray fluorescence element mapping reveals a positive correlation between Fe-Ti oxides and bulk-rock iron contents, suggesting that the formation of ferrogabbro is primarily attributed to the accumulation of Fe-Ti oxides. Petrographic characteristics combined with oxygen fugacity determinations indicate that the primitive magma had a low content of water and was moderately oxidized (ΔFMQ − 0.13 to ΔFMQ + 1.35). These conditions suppress the early crystallization of Fe-Ti oxides, thereby allowing for an enrichment of iron in the residual magma. Following the crystallization of plagioclase and pyroxenes, increased water content—evidenced by amphibole replacing pyroxenes—triggers extensive crystallization of Fe-Ti oxides. Due to their late-stage crystallization, these oxides do not settle within the magma, which possesses a high crystallinity (>50%) and consequently exhibits non-Newtonian fluid behavior. This results in the localized accumulation of Fe-Ti oxides and the formation of a ferrogabbro layer. However, the late-stage crystallization of Fe-Ti oxides also impedes the sinking and flow-sorting processes that are essential for the development of economically valuable Fe-Ti oxide layers. This may account for the lack of an economically valuable Fe-Ti oxide layer within the Dashanshu intrusion. | 
|---|---|
| Bibliography: | ObjectType-Article-1 SourceType-Scholarly Journals-1 ObjectType-Feature-2 content type line 14  | 
| ISSN: | 2075-163X 2075-163X  | 