Large matrix polymer solar cells fabricated by low cost air-brush spray deposition

In this paper,a 64 mm×64 mm matrix polymer solar cell(PSC) was fabricated by air-brush spray deposition.Although the open-circuit voltage(Voc) and the fill factor(FF) both need to be improved,the efficiency of matrix PSCs still reaches about 1.82%,and especially the current density achieves nearly 2...

Full description

Saved in:
Bibliographic Details
Published inOptoelectronics letters Vol. 11; no. 4; pp. 244 - 247
Main Author 陈征 邓振波 吕昭月 周茂杨 朱丽杰 殷月红 李熊
Format Journal Article
LanguageEnglish
Published Tianjin Tianjin University of Technology 01.07.2015
Subjects
Online AccessGet full text
ISSN1673-1905
1993-5013
DOI10.1007/s11801-015-5058-2

Cover

More Information
Summary:In this paper,a 64 mm×64 mm matrix polymer solar cell(PSC) was fabricated by air-brush spray deposition.Although the open-circuit voltage(Voc) and the fill factor(FF) both need to be improved,the efficiency of matrix PSCs still reaches about 1.82%,and especially the current density achieves nearly 20 m A/cm2.The results verify that air-brush spray deposition is a suitable method to prepare large area PSC devices,and the process we use in this paper can be easily transplanted to roll-to-roll production.
Bibliography:CHEN Zheng , DENG Zhen-bo , LU Zhao-yue, ZHOU Mao-yang, ZHU Li-jie, YIN Yue-hong, LI Xiong ( 1. National Teaching Center for Experimental Physics, Department of Physics, School of Science, Beijing Jiaotong University, Beijing 100044, China 2. Key Laboratory of Luminescence and Optical Information, Ministry of Education, Institute of Optoelectronic Technology, Beijing Jiaotong University, Beijing 100044, China 3. Department of Physics, School of Science, East China University of Science and Technology, Shanghai 200237, China)
12-1370/TN
In this paper,a 64 mm×64 mm matrix polymer solar cell(PSC) was fabricated by air-brush spray deposition.Although the open-circuit voltage(Voc) and the fill factor(FF) both need to be improved,the efficiency of matrix PSCs still reaches about 1.82%,and especially the current density achieves nearly 20 m A/cm2.The results verify that air-brush spray deposition is a suitable method to prepare large area PSC devices,and the process we use in this paper can be easily transplanted to roll-to-roll production.
brush spray prepare verify reaches annealing fabrication cathode controllable evaporation
ISSN:1673-1905
1993-5013
DOI:10.1007/s11801-015-5058-2