Long persistent and photostimulated luminescence properties of Sr2Al2SiO7:Eu2+/Tm3+ phosphors
A series of Sr2A12SiO7 phosphors with fixed Eu2+ concentration and various Tm3+ concentrations were synthesized via a high temperature solid state reaction. The structure and luminescence properties of the samples were characterized by X-ray powder diffraction (XRD), photoluminescence (PL) spectra,...
Saved in:
| Published in | Journal of rare earths Vol. 34; no. 1; pp. 1 - 6 |
|---|---|
| Main Author | |
| Format | Journal Article |
| Language | English |
| Published |
Elsevier B.V
2016
|
| Subjects | |
| Online Access | Get full text |
| ISSN | 1002-0721 2509-4963 |
| DOI | 10.1016/S1002-0721(14)60569-X |
Cover
| Summary: | A series of Sr2A12SiO7 phosphors with fixed Eu2+ concentration and various Tm3+ concentrations were synthesized via a high temperature solid state reaction. The structure and luminescence properties of the samples were characterized by X-ray powder diffraction (XRD), photoluminescence (PL) spectra, decay curves, thermoluminescence (TL) glow curves as well as the photostimu- lated luminescence (PSL) spectra. Sr2A12SiO7:Eu2+,Tm3+ phosphors exhibited strong green phosphorescence and photostimulated lu- minescence originating from 4f65d1-4f7 transition of Eu2+ after ultraviolet light stimulation. Deep traps were found by analyses on the phosphorescence decays and thermoluminescence spectra. It was also found that with increasing the time interval between UV excita- tion turn-off and stimulation turn-on, the photostimulated luminescence became stronger. This phenomenon resulted from the fact that the captured electron was retrapped by the deep traps. Compared with the Tm3+-free sample, it was found that the PSL intensity was strongly enhanced in Tm3+ eodoping samples. |
|---|---|
| Bibliography: | 11-2788/TF Sr2A12SiO7:Eu2+/Tm3+; long persistent; photostimulated luminescence; rare earths A series of Sr2A12SiO7 phosphors with fixed Eu2+ concentration and various Tm3+ concentrations were synthesized via a high temperature solid state reaction. The structure and luminescence properties of the samples were characterized by X-ray powder diffraction (XRD), photoluminescence (PL) spectra, decay curves, thermoluminescence (TL) glow curves as well as the photostimu- lated luminescence (PSL) spectra. Sr2A12SiO7:Eu2+,Tm3+ phosphors exhibited strong green phosphorescence and photostimulated lu- minescence originating from 4f65d1-4f7 transition of Eu2+ after ultraviolet light stimulation. Deep traps were found by analyses on the phosphorescence decays and thermoluminescence spectra. It was also found that with increasing the time interval between UV excita- tion turn-off and stimulation turn-on, the photostimulated luminescence became stronger. This phenomenon resulted from the fact that the captured electron was retrapped by the deep traps. Compared with the Tm3+-free sample, it was found that the PSL intensity was strongly enhanced in Tm3+ eodoping samples. |
| ISSN: | 1002-0721 2509-4963 |
| DOI: | 10.1016/S1002-0721(14)60569-X |