고분자 전해질막 수전해(PEMWE)용 SPEEK 막의 어닐링에 의한 내구성 향상

As Europe regulates perfluoroalkyl substances, efforts are underway to replace fluorinated polymer electrolyte membrane water electrolysis (PEMWE) membranes with hydrocarbon-based alternatives. However, hydrocarbon membranes like sulfonated poly ether ether ketone (SPEEK) face challenges of lower pe...

Full description

Saved in:
Bibliographic Details
Published in한국수소 및 신에너지학회 논문집 Vol. 36; no. 1; pp. 75 - 82
Main Authors 이미화, 유동근, 박권필, MIHWA LEE, DONGGEUN YOO, KWONPIL PARK
Format Journal Article
LanguageKorean
Published 한국수소및신에너지학회 01.02.2025
Subjects
Online AccessGet full text
ISSN1738-7264
2288-7407
DOI10.7316/JHNE.2025.36.1.75

Cover

Abstract As Europe regulates perfluoroalkyl substances, efforts are underway to replace fluorinated polymer electrolyte membrane water electrolysis (PEMWE) membranes with hydrocarbon-based alternatives. However, hydrocarbon membranes like sulfonated poly ether ether ketone (SPEEK) face challenges of lower performance and durability compared to fluorinated counterparts. This study focused on enhancing SPEEK membrane durability through annealing. SPEEK membranes were fabricated with varying annealing times (0-24 hours) at 140℃, and their properties were analyzed. As a result of annealing, the initial performance improved by 32-35%, and -S-O-S- crosslinking was formed through annealing, significantly enhancing the membrane durability. The SPEEK membrane annealed for 24 hours exhibited over six times greater durability compared to the non-annealed version, demonstrating potential as a viable hydrocarbon-based PEMWE membrane alternative.
AbstractList As Europe regulates perfluoroalkyl substances, efforts are underway to replace fluorinated polymer electrolyte membrane water electrolysis (PEMWE) membranes with hydrocarbon-based alternatives. However, hydrocarbon membranes like sulfonated poly ether ether ketone (SPEEK) face challenges of lower performance and durability compared to fluorinated counterparts. This study focused on enhancing SPEEK membrane durability through annealing. SPEEK membranes were fabricated with varying annealing times (0-24 hours) at 140℃, and their properties were analyzed. As a result of annealing, the initial performance improved by 32-35%, and -S-O-S- crosslinking was formed through annealing, significantly enhancing the membrane durability. The SPEEK membrane annealed for 24 hours exhibited over six times greater durability compared to the non-annealed version, demonstrating potential as a viable hydrocarbon-based PEMWE membrane alternative.
As Europe regulates perfluoroalkyl substances, efforts are underway to replace fluorinated polymer electrolyte membrane water electrolysis (PEMWE) membranes with hydrocarbon-based alternatives. However, hydrocarbon membranes like sulfonated poly ether ether ketone (SPEEK) face challenges of lower performance and durability compared to fluorinated counterparts. This study focused on enhancing SPEEK membrane durability through annealing. SPEEK membranes were fabricated with varying annealing times (0-24 hours) at 140℃, and their properties were analyzed. As a result of annealing, the initial performance improved by 32-35%, and -S-O-S- crosslinking was formed through annealing, significantly enhancing the membrane durability. The SPEEK membrane annealed for 24 hours exhibited over six times greater durability compared to the non-annealed version, demonstrating potential as a viable hydrocarbon-based PEMWE membrane alternative. KCI Citation Count: 0
Author 유동근
DONGGEUN YOO
박권필
이미화
MIHWA LEE
KWONPIL PARK
Author_xml – sequence: 1
  fullname: 이미화
– sequence: 2
  fullname: 유동근
– sequence: 3
  fullname: 박권필
– sequence: 4
  fullname: MIHWA LEE
– sequence: 5
  fullname: DONGGEUN YOO
– sequence: 6
  fullname: KWONPIL PARK
BackLink https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART003176165$$DAccess content in National Research Foundation of Korea (NRF)
BookMark eNotkE1LAlEUhi9hkJk_oN1sggpmuh9zP1yKTPlVSgltgmFmvMYwMoLTH7BcGG3caBIZbkKCNpH1o5zrf2jKVu97eJ9zDrzbIBV2QgnALoIGJ4gdlYtnloEhpgZhBjI43QBpjIXQuQl5CqQRJ4nHzNwC2SjyXQgRoohxlgZXy89Z_N1XL0NNzfqr0ULNB_H8XlODyXrer1unl9aBenrTLuqWVdGSVE0nmhov4odhPO-px2R1OlmNnrX4drH8elf9D201flV3vR2w2XLakcz-awY0jq1GoahXayelQr6qB4wK3eTQcaEk0vMIgch1PESxdIWUXtOFuRzzmMQiyUziSoE4FCaWDvEIoi3UZIxkwOH6bNht2YHn2x3H_9Prjh107fx5o2QjyASFpkjgvTUc-NGNb4fNqG2X85Xab30IUmpCmHzIkR8fy3pR
ContentType Journal Article
DBID JDI
ACYCR
DEWEY 621.042
DOI 10.7316/JHNE.2025.36.1.75
DatabaseName [Open Access] KoreaScience
Korean Citation Index
DatabaseTitleList

DeliveryMethod fulltext_linktorsrc
DocumentTitleAlternate Durability Increase of Polymer Electrolyte Membrane Water Electrolysis by Annealing of SPEEK Membrane
EISSN 2288-7407
EndPage 82
ExternalDocumentID oai_kci_go_kr_ARTI_10685048
JAKO202510554007089
GroupedDBID .UV
ALMA_UNASSIGNED_HOLDINGS
JDI
ACYCR
ID FETCH-LOGICAL-k658-470ab0e3ecc3301bac152eb8eecdb0996c6e28c3343be8170842ea3c315f1d663
ISSN 1738-7264
IngestDate Thu Jul 10 08:46:39 EDT 2025
Wed Apr 23 02:17:11 EDT 2025
IsDoiOpenAccess true
IsOpenAccess true
IsPeerReviewed false
IsScholarly false
Issue 1
Language Korean
LinkModel OpenURL
MergedId FETCHMERGED-LOGICAL-k658-470ab0e3ecc3301bac152eb8eecdb0996c6e28c3343be8170842ea3c315f1d663
Notes KISTI1.1003/JNL.JAKO202510554007089
OpenAccessLink http://click.ndsl.kr/servlet/LinkingDetailView?cn=JAKO202510554007089&dbt=JAKO&org_code=O481&site_code=SS1481&service_code=01
PageCount 8
ParticipantIDs nrf_kci_oai_kci_go_kr_ARTI_10685048
kisti_ndsl_JAKO202510554007089
PublicationCentury 2000
PublicationDate 2025-02
PublicationDateYYYYMMDD 2025-02-01
PublicationDate_xml – month: 02
  year: 2025
  text: 2025-02
PublicationDecade 2020
PublicationTitle 한국수소 및 신에너지학회 논문집
PublicationTitleAlternate Journal of hydrogen and new energy
PublicationYear 2025
Publisher 한국수소및신에너지학회
Publisher_xml – name: 한국수소및신에너지학회
SSID ssib001151676
ssib053377300
ssib044738289
ssib008451833
ssib012146272
Score 1.9106548
Snippet As Europe regulates perfluoroalkyl substances, efforts are underway to replace fluorinated polymer electrolyte membrane water electrolysis (PEMWE) membranes...
SourceID nrf
kisti
SourceType Open Website
Open Access Repository
StartPage 75
SubjectTerms 기계공학
Title 고분자 전해질막 수전해(PEMWE)용 SPEEK 막의 어닐링에 의한 내구성 향상
URI http://click.ndsl.kr/servlet/LinkingDetailView?cn=JAKO202510554007089&dbt=JAKO&org_code=O481&site_code=SS1481&service_code=01
https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART003176165
Volume 36
hasFullText 1
inHoldings 1
isFullTextHit
isPrint
ispartofPNX 한국수소및신에너지학회논문집, 2025, 36(1), , pp.75-82
journalDatabaseRights – providerCode: PRVHPJ
  databaseName: ROAD: Directory of Open Access Scholarly Resources
  customDbUrl:
  eissn: 2288-7407
  dateEnd: 99991231
  omitProxy: true
  ssIdentifier: ssib044738289
  issn: 1738-7264
  databaseCode: M~E
  dateStart: 20120101
  isFulltext: true
  titleUrlDefault: https://road.issn.org
  providerName: ISSN International Centre
link http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwvR1Na9RAdGjrxYsoKtaPEtABZdk1mUySmWOSptSW1oIVexCWTTIrZWUXanvxIFR7qHjppbWIlV6kCF7E6o_qpgf_gW9ekmarRaoHL2Ey8-bN-8jkvRcy7xFyy0vBjDKVgudm8TpPObwHnTStt5220PnOXRPPVs3MupMP-dSCszA0_GPgr6WV5biRPD_xXMm_aBX6QK_6lOxfaPYIKXRAG_QLV9AwXE-lYxr5NLCpb9IooIFLBadRSGVEpVnTLRjQXeNUOjTAMd-jQmho3ZAIBPdSnADNxFw08yiiTCJSn_qy9mAuiqZrR_NxAOAFIpIuLhJQEQABJZCFQ15JEoIXi8gQUQmG84AVh_ohksRpYNUQyqW-g102zYuulJ70EY5y5vgxZgRII0SxAFcT2BOgoApicGGOwsilYpYIJTb8YroAWWADKAtKYGnpJ1NXqQH2qk8pBX-5EPwJhB_XCCU_BhIWGgO69GpAvkeDsAJBooEUPZKzgZTlRe7KTzTMKf_qLjbVfxDIgAXzwIJ5LE8N31DYx5jQSWPz8sKFpcrr1ZQ-DzvJmuqiZrpQ-ORs1NBsNWy3YTXKiYOZy3_xKI7lLu8ki80nvWZnqQkR2r2mZcIbAMzGMDnDwBDraiszL6LKgwcP1B3wkAV3LFFFJJauQ8-qo96cA7usKpgAwYunKzDgMehCEPm_DJqZu7-xAiGpjtMWwbPsLrUHPMv58-RcERIafr6_L5ChTu8ieXzwdbf_fS37sGFku2uHm_vZ3np_77WRrW_n97dxd97J3n0ycFcaMJrtbBvZ1n7_zUZ_bzV7C1N3tg833xv9l_sH3z5na1-Mw62P2avVS2R-IpoPJ-tFJZR6ByKEOvfMVmwqG163NhjkuJWA161ioVSSxhDiuYmrmIAxbsdKZ9wUnKmWndiW07ZSiCkuk5Fur6uuEAMCtESfYGyBY8FFO25x2VK2qYSb2ELFySgZQ4E0u-mzp80pf_q-Fpeuost1ZjAhR8lNkBRq9Q_avXoqqGvkbLVdrpOR5aUVdQN8_OV4DJ-Kn4KTvik
linkProvider ISSN International Centre
openUrl ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=%EA%B3%A0%EB%B6%84%EC%9E%90+%EC%A0%84%ED%95%B4%EC%A7%88%EB%A7%89+%EC%88%98%EC%A0%84%ED%95%B4%28PEMWE%29%EC%9A%A9+SPEEK+%EB%A7%89%EC%9D%98+%EC%96%B4%EB%8B%90%EB%A7%81%EC%97%90+%EC%9D%98%ED%95%9C+%EB%82%B4%EA%B5%AC%EC%84%B1+%ED%96%A5%EC%83%81&rft.jtitle=%ED%95%9C%EA%B5%AD%EC%88%98%EC%86%8C%EB%B0%8F%EC%8B%A0%EC%97%90%EB%84%88%EC%A7%80%ED%95%99%ED%9A%8C%EB%85%BC%EB%AC%B8%EC%A7%91%2C+36%281%29&rft.au=%EC%9D%B4%EB%AF%B8%ED%99%94&rft.au=%EC%9C%A0%EB%8F%99%EA%B7%BC&rft.au=%EB%B0%95%EA%B6%8C%ED%95%84&rft.date=2025-02-01&rft.pub=%ED%95%9C%EA%B5%AD%EC%88%98%EC%86%8C%EB%B0%8F%EC%8B%A0%EC%97%90%EB%84%88%EC%A7%80%ED%95%99%ED%9A%8C&rft.issn=1738-7264&rft.eissn=2288-7407&rft.spage=75&rft.epage=82&rft_id=info:doi/10.7316%2FJHNE.2025.36.1.75&rft.externalDBID=n%2Fa&rft.externalDocID=oai_kci_go_kr_ARTI_10685048
thumbnail_l http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1738-7264&client=summon
thumbnail_m http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1738-7264&client=summon
thumbnail_s http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1738-7264&client=summon