박판주조법으로 제조한 Al-0.6Mg-1.2Si 합금판재의 소부경화특성
The effect of pre-aging treatment on the microstructure and mechanical properties of Al-0.6Mg-1.2Si aluminum alloy sheets fabricated by twin roll casting (TRC) was investigated. It was observed that two kinds of nanoclusters, cluster(1) and cluster(2), play an important role in the bake-hardening pr...
Saved in:
Published in | 대한금속·재료학회지, 55(12) Vol. 55; no. 12; pp. 853 - 861 |
---|---|
Main Authors | , , , , , , , , , |
Format | Journal Article |
Language | Korean |
Published |
대한금속재료학회
05.12.2017
대한금속·재료학회 |
Subjects | |
Online Access | Get full text |
ISSN | 1738-8228 2288-8241 |
DOI | 10.3365/KJMM.2017.55.12.853 |
Cover
Abstract | The effect of pre-aging treatment on the microstructure and mechanical properties of Al-0.6Mg-1.2Si aluminum alloy sheets fabricated by twin roll casting (TRC) was investigated. It was observed that two kinds of nanoclusters, cluster(1) and cluster(2), play an important role in the bake-hardening properties of Al-Mg-Si aluminum alloy. The hardness of the TRC Al-0.6Mg-1.2Si alloy sheets was continuously increased up to 48 h by natural-aging, and the highest yield strength value was about 146 MPa. The yield strength was 280 MPa after bake-hardening at 180 ℃ for 30 min immediately after quenching, whereas the yield strength was 172 MPa when natural-aging proceeded for about 1 week before bake-hardening. This result is due to fact that cluster(1) is formed during natural-aging at room temperature and has detrimental effects on bake-hardening. On the other hand, when pre-aged at 150 ℃ for 10 min, cluster(2) predominantly formed and promoted the precipitation of β″ phase. The yield strength was 256 MPa after bake-hardening, which indicates that the pre-aging treatment is an effective method, and also depresses the negative effects of natural-aging and promotes β″ precipitation. The Al-Mg-Si aluminum alloy sheets fabricated by twin roll casting method exhibited mechanical properties equal to or higher than those of the direct-chill (DC) casting sheets despite the simplified manufacturing process.
(Received July 10, 2017; Accepted September 15, 2017) |
---|---|
AbstractList | The effect of pre-aging treatment on the microstructure and mechanical properties of Al-0.6Mg-1.2Si aluminum alloy sheets fabricated by twin roll casting (TRC) was investigated. It was observed that two kinds of nanoclusters, cluster(1) and cluster(2), play an important role in the bake-hardening properties of Al-Mg-Si aluminum alloy. The hardness of the TRC Al-0.6Mg-1.2Si alloy sheets was continuously increased up to 48 h by natural-aging, and the highest yield strength value was about 146 MPa. The yield strength was 280 MPa after bake-hardening at 180 ℃ for 30 min immediately after quenching, whereas the yield strength was 172 MPa when natural-aging proceeded for about 1 week before bake-hardening. This result is due to fact that cluster(1) is formed during natural-aging at room temperature and has detrimental effects on bake-hardening. On the other hand, when pre-aged at 150 ℃ for 10 min, cluster(2) predominantly formed and promoted the precipitation of β″ phase. The yield strength was 256 MPa after bake-hardening, which indicates that the pre-aging treatment is an effective method, and also depresses the negative effects of natural-aging and promotes β″ precipitation. The Al-Mg-Si aluminum alloy sheets fabricated by twin roll casting method exhibited mechanical properties equal to or higher than those of the direct-chill (DC) casting sheets despite the simplified manufacturing process.
(Received July 10, 2017; Accepted September 15, 2017) The effect of pre-aging treatment on the microstructure and mechanical properties of Al-0.6Mg-1.2Si aluminum alloy sheets fabricated by twin roll casting (TRC) was investigated. It was observed that two kinds of nanoclusters, cluster(1) and cluster(2), play an important role in the bake-hardening properties of Al-Mg-Si aluminum alloy. The hardness of the TRC Al-0.6Mg-1.2Si alloy sheets was continuously increased up to 48 h by natural-aging, and the highest yield strength value was about 146 MPa. The yield strength was 280 MPa after bake-hardening at 180 ℃ for 30 min immediately after quenching, whereas the yield strength was 172 MPa when natural-aging proceeded for about 1 week before bake-hardening. This result is due to fact that cluster(1) is formed during natural-aging at room temperature and has detrimental effects on bake-hardening. On the other hand, when pre-aged at 150 ℃ for 10 min, cluster(2) predominantly formed and promoted the precipitation of β″ phase. The yield strength was 256 MPa after bake-hardening, which indicates that the pre-aging treatment is an effective method, and also depresses the negative effects of natural-aging and promotes β″ precipitation. The Al-Mg-Si aluminum alloy sheets fabricated by twin roll casting method exhibited mechanical properties equal to or higher than those of the direct-chill (DC) casting sheets despite the simplified manufacturing process. KCI Citation Count: 2 |
Author | Hyoung-wook Kim Gi-cheol Ju 주기철 김민석 Min-seok Kim 김형욱 Yun-soo Lee 김양도 Yang-do Kim 이윤수 |
Author_xml | – sequence: 1 fullname: 주기철 – sequence: 2 fullname: Gi-cheol Ju – sequence: 3 fullname: 이윤수 – sequence: 4 fullname: Yun-soo Lee – sequence: 5 fullname: 김민석 – sequence: 6 fullname: Min-seok Kim – sequence: 7 fullname: 김형욱 – sequence: 8 fullname: Hyoung-wook Kim – sequence: 9 fullname: 김양도 – sequence: 10 fullname: Yang-do Kim |
BackLink | https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART002288374$$DAccess content in National Research Foundation of Korea (NRF) |
BookMark | eNotjL1Kw1AAhS9SwVr7BF2yOiTe_3szluJPtUXU7iExuSWktpJMbg4iIh0cDChEsTgJDrWDKNQXam7ewdY6fefAOd86KPUH_QCAGoIWIZxtHey32xaGSFiMWQhbkpEVUMZYSlNiikqgjARZZCzXQDVJQg9CjjlmFJbBUT5Oi-Gdfp3q0TifpDqb5qPM0C_ZvBdpZtR7JrR4u2siC5-ERpG-zb5uFo_nd_30YOjrYf55OZv8FI_3xe23vvrYAKvK7SVB9Z8V0NnZ7jT2zNbhbrNRb5kRo8ikHmYehT52Xa6gy3jgY4gVQoGigkmPU24jolSgiK8UE67nY2nbtmR2ICjzSQVsLrX9WDnRaegM3PCP3YETxU79uNN0MKJQzDUVUFtuozBJnPM4PHPjC4cwJgRF5Be-l3L0 |
ContentType | Journal Article |
DBID | HZB Q5X ACYCR |
DOI | 10.3365/KJMM.2017.55.12.853 |
DatabaseName | KISS Korean Studies Information Service System (KISS) B-Type Korean Citation Index |
DatabaseTitleList | |
DeliveryMethod | fulltext_linktorsrc |
DocumentTitleAlternate | 박판주조법으로 제조한 Al-0.6Mg-1.2Si 합금판재의 소부경화특성 Bake-hardening Properties of Al-0.6Mg-1.2Si Alloy Sheets Fabricated by Twin Roll Casting |
EISSN | 2288-8241 |
EndPage | 861 |
ExternalDocumentID | oai_kci_go_kr_ARTI_2140791 3557741 |
GroupedDBID | ALMA_UNASSIGNED_HOLDINGS HZB M~E Q5X ACYCR |
ID | FETCH-LOGICAL-k541-4b25b40d2aa6f0a56ed202f11ef4758b646913ffef3dff57abd28999859e745d3 |
ISSN | 1738-8228 |
IngestDate | Tue Nov 21 21:03:10 EST 2023 Thu Jan 16 03:38:52 EST 2025 |
IsPeerReviewed | true |
IsScholarly | true |
Issue | 12 |
Language | Korean |
LinkModel | OpenURL |
MergedId | FETCHMERGED-LOGICAL-k541-4b25b40d2aa6f0a56ed202f11ef4758b646913ffef3dff57abd28999859e745d3 |
Notes | The Korean Institute of Metals and Materials |
PageCount | 9 |
ParticipantIDs | nrf_kci_oai_kci_go_kr_ARTI_2140791 kiss_primary_3557741 |
PublicationCentury | 2000 |
PublicationDate | 20171205 |
PublicationDateYYYYMMDD | 2017-12-05 |
PublicationDate_xml | – month: 12 year: 2017 text: 20171205 day: 05 |
PublicationDecade | 2010 |
PublicationTitle | 대한금속·재료학회지, 55(12) |
PublicationTitleAlternate | 대한금속재료학회지 |
PublicationYear | 2017 |
Publisher | 대한금속재료학회 대한금속·재료학회 |
Publisher_xml | – name: 대한금속재료학회 – name: 대한금속·재료학회 |
SSID | ssib006262540 ssib022232341 ssib044734076 ssib023167440 ssib036264765 ssib001148846 ssib002806993 ssib014806100 ssib005195854 |
Score | 2.0659635 |
Snippet | The effect of pre-aging treatment on the microstructure and mechanical properties of Al-0.6Mg-1.2Si aluminum alloy sheets fabricated by twin roll casting (TRC)... |
SourceID | nrf kiss |
SourceType | Open Website Publisher |
StartPage | 853 |
SubjectTerms | aluminium bake-hardening precipitation twin roll casting yield strength 재료공학 |
Title | 박판주조법으로 제조한 Al-0.6Mg-1.2Si 합금판재의 소부경화특성 |
URI | https://kiss.kstudy.com/ExternalLink/Ar?key=3557741 https://www.kci.go.kr/kciportal/ci/sereArticleSearch/ciSereArtiView.kci?sereArticleSearchBean.artiId=ART002288374 |
Volume | 55 |
hasFullText | 1 |
inHoldings | 1 |
isFullTextHit | |
isPrint | |
ispartofPNX | 대한금속·재료학회지, 2017, 55(12), 533, pp.853-861 |
journalDatabaseRights | – providerCode: PRVHPJ databaseName: ROAD: Directory of Open Access Scholarly Resources customDbUrl: eissn: 2288-8241 dateEnd: 99991231 omitProxy: true ssIdentifier: ssib044734076 issn: 1738-8228 databaseCode: M~E dateStart: 20070101 isFulltext: true titleUrlDefault: https://road.issn.org providerName: ISSN International Centre |
link | http://utb.summon.serialssolutions.com/2.0.0/link/0/eLvHCXMwrV3Nb9MwFLe2ceGCQAMxvlQhfJoyEsdO7GPSBsagCMSQxilqGmeaKrVoHxcOiANCCO3AgUogFcTECYnD2AGBNP6hNf0feM8pTTbtAIhL6tq_9_zx7Pg923km5JojslRrsE7ARBYWb3NmtYRILOhNLGFtDbHmgOxdb_EhX1oRK1PT9yqnlrY2k4X2k2O_K_kXqUIcyBW_kv0LyU6YQgSEQb7wBAnD849kTKOQhjZVgkYNKutU2TSq08ClYd0EHExFDDMYANRNUohJqj5vQDbGlugGQhV--WLZC15z1QLz9sHa_DghUDQKaCiplIfyVBENDBcFMGkYSw-TMXcPj1MgGaNhwzBSVHFDD5HKgDkNnaqijIRALssSVTIumDcqGYdYa8yuACsTCEwM1MyncrIrU2khwy805YeiBRPIzTULunIPrzqrUkHVQj5uxcAEoCxqchT40VbX2uj15u9oXV1KgekZj6WISef_XzWrTCc-TCeggsnqfFO4Jf49rlhl9pCF3-Sjs5rreugA5PZSs4lnEf0FIXAJe4w-4i4c9EfQ6J1pcoL5nod3ejSfRqWCDNav5If31VXlDQ3mLROl9x9Ag75XOnBEZZK5pQLN0I8CL_Ho24j75b45577LbXPD46QpCtdfWKfrx9QINCMwnDZA0-uuZxVNb_k0OTU20WpBMd7OkKlOb5bcH-72R9uv80_7-c7ucK-fD_aHO4Na_nEA_0f9Qe3weKmN-p8Pvr9Eig9f8vdva_mL7eG3Zwd7P0fv3oxe_ciffz1Llm9Ey_VFa3wdidUR3LF4wkTC7ZS1Wl5mt4SnU2azzHF0xsHoTjzuKcfNMp25aZYJv5WkuJihpFDa5yJ1z5GZbq-rz5Oa9Hjbb2thu1rzrJVKsKt84Jy4ieBaijkyi40QPy4czsRjmc6Rq9Aocae9FqNTePxd7cWd9RhM31sxc6CllXPheNqL5GTZ4y-Rmc31LX0Z1OnN5IrpIb8Azp2ZrQ |
linkProvider | ISSN International Centre |
openUrl | ctx_ver=Z39.88-2004&ctx_enc=info%3Aofi%2Fenc%3AUTF-8&rfr_id=info%3Asid%2Fsummon.serialssolutions.com&rft_val_fmt=info%3Aofi%2Ffmt%3Akev%3Amtx%3Ajournal&rft.genre=article&rft.atitle=%EB%B0%95%ED%8C%90%EC%A3%BC%EC%A1%B0%EB%B2%95%EC%9C%BC%EB%A1%9C+%EC%A0%9C%EC%A1%B0%ED%95%9C+Al-0.6Mg-1.2Si+%ED%95%A9%EA%B8%88%ED%8C%90%EC%9E%AC%EC%9D%98+%EC%86%8C%EB%B6%80%EA%B2%BD%ED%99%94%ED%8A%B9%EC%84%B1&rft.jtitle=%EB%8C%80%ED%95%9C%EA%B8%88%EC%86%8D%EC%9E%AC%EB%A3%8C%ED%95%99%ED%9A%8C%EC%A7%80&rft.au=%EC%A3%BC%EA%B8%B0%EC%B2%A0&rft.au=Gi-cheol+Ju&rft.au=%EC%9D%B4%EC%9C%A4%EC%88%98&rft.au=Yun-soo+Lee&rft.date=2017-12-05&rft.pub=%EB%8C%80%ED%95%9C%EA%B8%88%EC%86%8D%EC%9E%AC%EB%A3%8C%ED%95%99%ED%9A%8C&rft.issn=1738-8228&rft.volume=55&rft.issue=12&rft.spage=853&rft_id=info:doi/10.3365%2FKJMM.2017.55.12.853&rft.externalDocID=3557741 |
thumbnail_l | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/lc.gif&issn=1738-8228&client=summon |
thumbnail_m | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/mc.gif&issn=1738-8228&client=summon |
thumbnail_s | http://covers-cdn.summon.serialssolutions.com/index.aspx?isbn=/sc.gif&issn=1738-8228&client=summon |