Thermomechanical treatment of super high strength Cu-8.0Ni-1.8Si alloy

The microstructures and properties of Cu-8.0Ni-1.8Si alloy subjected to different heat treatments were examined by mechanical and electrical properties measurements, optical and transmission electron microscopes observation. The results show that the precipitation process during aging can be acceler...

Full description

Saved in:
Bibliographic Details
Published inTransactions of Nonferrous Metals Society of China Vol. 17; no. A02; pp. 1076 - 1080
Main Author 潘志勇 汪明朴 李周 肖柱 陈畅
Format Journal Article
LanguageEnglish
Published 01.11.2007
Subjects
Online AccessGet full text
ISSN1003-6326

Cover

More Information
Summary:The microstructures and properties of Cu-8.0Ni-1.8Si alloy subjected to different heat treatments were examined by mechanical and electrical properties measurements, optical and transmission electron microscopes observation. The results show that the precipitation process during aging can be accelerated by the cold deforming before aging. As the Cu-8.0Ni-1.8Si alloy is subjected to solution treatment at 970 ℃ for 4 h, cold rolling to 60% reduction, and then aging at 450 ℃ for 60 min, its properties are σb=1 050 MPa, σ0.2=786 MPa, δ=3.2% and conductivity 27.9%(IACS). The strengthening mechanisms of the alloy include spinodal decomposition strengthening, ordering strengthening and precipitation strengthening. The precipitation of the alloy is nano-scale Ni2Si phase.
Bibliography:Cu-8.0Ni- 1.8Si alloy
43-1239/TG
thermomechanical treatment
ordering
Cu-8.0Ni- 1.8Si alloy; thermomechanical treatment; spinodal decomposition; ordering