Mechanism of micro-waviness induced KH2PO4 crystal laser damage and the corresponding vibration source

The low laser induced damage threshold of the KH2PO4 crystal seriously restricts the output power of inertial confinement fusion.The micro-waviness on the KH2PO4 surface processed by single point diamond turning has a significant influence on the damage threshold.In this paper,the influence of micro...

Full description

Saved in:
Bibliographic Details
Published in中国物理B:英文版 Vol. 21; no. 5; pp. 34 - 42
Main Author 李明全 陈明君 安晨辉 周炼 程健 肖勇 姜伟
Format Journal Article
LanguageEnglish
Published 01.05.2012
Subjects
Online AccessGet full text
ISSN1674-1056
2058-3834
DOI10.1088/1674-1056/21/5/050301

Cover

More Information
Summary:The low laser induced damage threshold of the KH2PO4 crystal seriously restricts the output power of inertial confinement fusion.The micro-waviness on the KH2PO4 surface processed by single point diamond turning has a significant influence on the damage threshold.In this paper,the influence of micro-waviness on the damage threshold of the KH2PO4 crystal and the chief sources introducing the micro-waviness are analysed based on the combination of the Fourier modal theory and the power spectrum density method.Research results indicate that among the sub-wavinesses with different characteristic spatial frequencies there exists the most dangerous frequency which greatly reduces the damage threshold,although it may not occupy the largest proportion in the original surface.The experimental damage threshold is basically consistent with the theoretical calculation.For the processing parameters used,the leading frequency of micro-waviness which causes the damage threshold to decrease is between 350-1 μm-1 and 30-1 μm-1,especially between 90-1 μm-1 and 200-1 μm-1.Based on the classification study of the time frequencies of microwaviness,we find that the axial vibration of the spindle is the chief source introducing the micro-waviness,nearly all the leading frequencies are related to the practical spindle frequency(about 6.68 Hz,400 r/min) and a special middle frequency(between 1.029 Hz and 1.143 Hz).
Bibliography:The low laser induced damage threshold of the KH2PO4 crystal seriously restricts the output power of inertial confinement fusion.The micro-waviness on the KH2PO4 surface processed by single point diamond turning has a significant influence on the damage threshold.In this paper,the influence of micro-waviness on the damage threshold of the KH2PO4 crystal and the chief sources introducing the micro-waviness are analysed based on the combination of the Fourier modal theory and the power spectrum density method.Research results indicate that among the sub-wavinesses with different characteristic spatial frequencies there exists the most dangerous frequency which greatly reduces the damage threshold,although it may not occupy the largest proportion in the original surface.The experimental damage threshold is basically consistent with the theoretical calculation.For the processing parameters used,the leading frequency of micro-waviness which causes the damage threshold to decrease is between 350-1 μm-1 and 30-1 μm-1,especially between 90-1 μm-1 and 200-1 μm-1.Based on the classification study of the time frequencies of microwaviness,we find that the axial vibration of the spindle is the chief source introducing the micro-waviness,nearly all the leading frequencies are related to the practical spindle frequency(about 6.68 Hz,400 r/min) and a special middle frequency(between 1.029 Hz and 1.143 Hz).
Li Ming-Quan ,Chen Ming-Jun ,An chen-Hui ,Zhou Lian ,Cheng Jian ,Xiao Yong,and Jiang Wei a) Center for Precision Engineering,Harbin Institute of Technology,Harbin 150001,China b) Chengdu Fine Optical Engineering Research Center,Chengdu 610041,China
laser induced damage threshold; micro-waviness; Fourier modal theory; power spectrum density
11-5639/O4
ISSN:1674-1056
2058-3834
DOI:10.1088/1674-1056/21/5/050301