Corrosion behaviour of stainless steel, nickel base alloy and titanium weldments in chlorination and chlorine dioxide bleaching

This publication presents an overview of a decade-long series of programs which exposed welded coupon and full diameter pipe in chlorination and chlorine dioxide bleaching equipment. Findings have guided procedures for the fabrication and post fabrication clean-up of over 75 6% Mo stainless steel wa...

Full description

Saved in:
Bibliographic Details
Main Authors: Tuthill, Arthur H., (Author), Avery, Richard E., (Author), Garner, Andrew, (Author)
Format: eBook
Language: English
Published: Toronto, Ont. : Nickel Development Institute, 1992.
Series: Technical series (Nickel Development Institute (Canada)) ; no. 14 026.
Subjects:
ISBN: 9781523131075
1523131071
Physical Description: 1 online resource (20 pages) : illustrations

Cover

Table of contents

LEADER 02775cam a2200409 i 4500
001 kn-on1255595075
003 OCoLC
005 20240717213016.0
006 m o d
007 cr cn|||||||||
008 210609s1992 onca ob 000 0 eng d
040 |a HUA  |b eng  |e rda  |e pn  |c HUA  |d HUA  |d OCLCO  |d OCLCF  |d OCLCO  |d UAB  |d OCLCL 
020 |a 9781523131075  |q (electronic bk.) 
020 |a 1523131071  |q (electronic bk.) 
035 |a (OCoLC)1255595075 
100 1 |a Tuthill, Arthur H.,  |e author. 
245 1 0 |a Corrosion behaviour of stainless steel, nickel base alloy and titanium weldments in chlorination and chlorine dioxide bleaching /  |c Arthur H. Tuthill, Richard E. Avery, and Andrew Garner. 
264 1 |a Toronto, Ont. :  |b Nickel Development Institute,  |c 1992. 
300 |a 1 online resource (20 pages) :  |b illustrations 
336 |a text  |b txt  |2 rdacontent 
337 |a computer  |b c  |2 rdamedia 
338 |a online resource  |b cr  |2 rdacarrier 
490 1 |a NiDI reprint series ;  |v no. 14 026 
500 |a "Reprinted with permission from Proceedings of the Technical Association of the Pulp and Paper Industry, TAPPI, 7th International Symposium on Corrosion in the Pulp and Paper Industry, Orlando, FL, 1992" 
504 |a Includes bibliographical references. 
506 |a Plný text je dostupný pouze z IP adres počítačů Univerzity Tomáše Bati ve Zlíně nebo vzdáleným přístupem pro zaměstnance a studenty 
520 |a This publication presents an overview of a decade-long series of programs which exposed welded coupon and full diameter pipe in chlorination and chlorine dioxide bleaching equipment. Findings have guided procedures for the fabrication and post fabrication clean-up of over 75 6% Mo stainless steel washers. Findings are also applicable to 6% Mo, nickel base alloy, clad nickel base alloy, titanium and plastic-lined piping for bleach plants. Guidelines for procurement and fabrication of piping materials are included. Applicability to mixer-to-tower, tower-to-vat and filtrate piping sections is reported. 
590 |a Knovel  |b Knovel (All titles) 
650 0 |a Alloys  |x Corrosion. 
650 0 |a Bleaching industry  |x Equipment and supplies  |x Corrosion. 
655 7 |a elektronické knihy  |7 fd186907  |2 czenas 
655 9 |a electronic books  |2 eczenas 
700 1 |a Avery, Richard E.,  |e author. 
700 1 |a Garner, Andrew,  |e author. 
776 0 8 |i Print version:  |a Tuthill, Arthur H.  |t Corrosion behaviour of stainless steel, nickel base alloy and titanium weldments in chlorination and chlorine dioxide bleaching 
830 0 |a Technical series (Nickel Development Institute (Canada)) ;  |v no. 14 026. 
856 4 0 |u https://proxy.k.utb.cz/login?url=https://app.knovel.com/hotlink/toc/id:kpCBSSNBAB/corrosion-behaviour-of?kpromoter=marc  |y Full text