Covers the mechanical behavior of ceramic matrix composites at elevated temperatures. Topics include both short-term behavior (strength, fracture toughness, and R-curve behavior) and long-term behavior (creep, creep-fatigue, delayed failure, and lifetime).

Saved in:
Bibliographic Details
Other Authors: Nair, Shantikumar Vasudevan, 1953-, Jakus, Karl.
Format: eBook
Language: English
Published: Boston : Butterworth-Heinemann, c1995.
Subjects:
ISBN: 9781591243151
9780750693998
9780080523880
9781281072795
Physical Description: 1 online zdroj (x, 558 p.) : ill.

Cover

Table of contents

LEADER 02535cam a2200421 a 4500
001 77281
003 CZ ZlUTB
005 20200530180901.0
006 m o d
007 cr |n
008 020403s1995 maua sb 001 0 eng d
020 |a 9781591243151  |q (ebook) 
020 |a 9780750693998 
020 |a 9780080523880  |q (ebook) 
020 |a 9781281072795 
035 |a (OCoLC)50266833  |z (OCoLC)162129737  |z (OCoLC)181087459  |z (OCoLC)624380502  |z (OCoLC)647688735  |z (OCoLC)648584568  |z (OCoLC)823830555  |z (OCoLC)823900261  |z (OCoLC)824091526  |z (OCoLC)824139752 
040 |a KNOVL  |b eng  |c KNOVL  |d TEF  |d OCLCG  |d OCLCQ  |d OPELS  |d OCLCE  |d N$T  |d YDXCP  |d IDEBK  |d E7B  |d MERUC  |d KNOVL  |d OCLCF  |d OCLCO  |d KNOVL  |d ZCU 
245 0 0 |a High temperature mechanical behavior of ceramic composites  |h [elektronický zdroj] /  |c edited by Shanti V. Nair and Karl Jakus. 
260 |a Boston :  |b Butterworth-Heinemann,  |c c1995. 
300 |a 1 online zdroj (x, 558 p.) :  |b ill. 
336 |a text  |b txt  |2 rdacontent 
337 |a počítač  |b c  |2 rdamedia 
338 |a online zdroj  |b cr  |2 rdacarrier 
520 |a Covers the mechanical behavior of ceramic matrix composites at elevated temperatures. Topics include both short-term behavior (strength, fracture toughness, and R-curve behavior) and long-term behavior (creep, creep-fatigue, delayed failure, and lifetime). 
504 |a Includes bibliographical references and index. 
505 0 |a Introduction; Interfaces; Residual stresses; Fibre properties; Matrix cracking in unidirectional materials; Matrix cracking in 2-D materials; Stress redistribution; Fatigue, creep, challenges and opportunities. 
590 |a Knovel Library  |b ACADEMIC - Ceramics & Ceramic Engineering 
506 |a Plný text je dostupný pouze z IP adres počítačů Univerzity Tomáše Bati ve Zlíně nebo vzdáleným přístupem pro zaměstnance a studenty univerzity 
650 0 |a Ceramic-matrix composites  |x Mechanical properties. 
650 0 |a Materials at high temperatures. 
655 7 |a elektronické knihy  |7 fd186907  |2 czenas 
655 9 |a electronic books  |2 eczenas 
700 1 |a Nair, Shantikumar Vasudevan,  |d 1953- 
700 1 |a Jakus, Karl. 
776 0 8 |i Print version:  |t High temperature mechanical behavior of ceramic composites.  |d Boston : Butterworth-Heinemann, c1995  |z 0750693991  |w (DLC) 95009951  |w (OCoLC)32132537 
856 4 0 |u https://proxy.k.utb.cz/login?url=http://app.knovel.com/hotlink/toc/id:kpHTMBCC03/high_temperature_mechanical_behavior_of_ceramic_composites  |y Plný text 
992 |a BK  |c KNOVEL 
999 |c 77281  |d 77281